Adhesive Preparation
Raw Material Blending: Raw materials-such as acrylic monomers, initiators, and tackifying resins-are weighed according to precise ratios, with measurement errors controlled to ≤0.5%.
Emulsification: The mixture is stirred in an emulsification tank at 50–60°C for 2–3 hours to fully disperse the monomers and form a stable emulsion.
Synthesis & Maturation: The emulsion is transferred to a reactor for heating and polymerization; the adhesive viscosity is adjusted to 3,000–5,000 mPa·s (at 25°C). Upon completion, parameters such as appearance, viscosity, and shear strength are tested; substandard batches are discarded.
Substrate Pre-treatment
BOPP film (23–28 μm thick) is selected. High-pressure corona treatment is applied to enhance surface tension-ensuring firm adhesion of subsequent adhesives and inks-while removing surface impurities and ensuring the substrate remains flat and wrinkle-free.
Printing Process (For Custom Orders)
For tapes requiring logos or warning text, printing is performed prior to adhesive application:
Flexographic printing is used for simple, small-batch designs due to low costs and flexible plate changes; rotogravure printing is used for complex, high-definition designs to achieve superior color saturation.
After printing, the tape passes through a drying unit to rapidly evaporate ink solvents, preventing smudging or blurring of the design.